loading page

Thermo-mechanical fatigue behaviour of an additively manufactured nickel-based superalloy: experiments and crystal plasticity modeling
  • +6
  • Lu Zhang,
  • Liujun Lu,
  • Y. Z. Wang,
  • Weilong Li,
  • Z. W. Yu,
  • Xingling Luo,
  • Rong Jiang,
  • Liguo Zhao,
  • Yingdong Song
Lu Zhang
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering

Corresponding Author:luzhang@nuaa.edu.cn

Author Profile
Liujun Lu
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering
Author Profile
Y. Z. Wang
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering
Author Profile
Weilong Li
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering
Author Profile
Z. W. Yu
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering
Author Profile
Xingling Luo
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering
Author Profile
Rong Jiang
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering
Author Profile
Liguo Zhao
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering
Author Profile
Yingdong Song
Nanjing University of Aeronautics and Astronautics College of Energy and Power Engineering
Author Profile

Abstract

Thermo-mechanical fatigue (TMF) tests were carried out for additively manufactured nickel-based superalloy GH4169 with different printing directions. Selective-laser-melting specimens were subjected to a mechanical strain amplitude of 0.8% at temperature 350-650°C, under both in-phase (IP) and out-of-phase (OP) conditions. The research results indicate that the TMF life of horizontally printed samples is significantly longer than that of vertically printed samples. Furthermore, the TMF life under OP conditions is higher than that under IP conditions, with the isothermal fatigue life falling between the two. A crystal plasticity finite element model was established to simulate TMF cyclic deformation, taking into account the influence of plastic dissipation energy. The developed model is able to capture the features of asymmetry of stress-strain responses and initial hardening followed by softening. It was found that the strain distribution pattern is closely correlated with the shear bands generated by crystal slip, and some grains undergo premature softening.